This paper details the development of Hiduron® 220 (formerly Marinel 220) – specifically the control of the microstructure to achieve optimum mechanical properties. This alloy provides improved performance over Cu-Ni-Sn, particularly with respect to hydrogen embrittlement and stress corrosion cracking.